Silicon Nitride (Si3N4) has the most versatile combination of mechanical, thermal, and electrical properties of any advanced ceramic material. It is a high performance advanced ceramic that is extremely hard and has exceptional thermal shock and impact resistance. It surpasses the high temperature capabilities of most metals and has a superior combination of creep and oxidation resistance. Additionally, its low thermal conductivity and high wear resistance make it an excellent material that can withstand the toughest of conditions in the most demanding industrial applications. Silicon Nitride is an excellent choice when high-temperature and high-load abilities are needed.
Silicon nitride ceramic square structural parts are very wear-resistant because of their superb hardness and self-wetting properties. In addition, silicon nitride ceramic does not react with other inorganic acids except hydrofluoric acid, and is highly resistant to corrosion. Moreover, it has excellent resistance to thermal shock and will not rupture when heated to 1000°C in air and then rapidly cooled.
Silicon Nitride Applications | |
|
Property | Item | Data | Unit |
Mechanical Characteristics | Color | Black/Grey | - |
Density | 3.2 | g/cm3 | |
Bending Strength | 750 | MPa | |
Compressive Strength | 3800 | MPa | |
Elastic Modulus | 290 | GPa | |
Fracture Toughness | 7 | MPa m1/2 | |
Weber Coefficient | 15 | m | |
Vickers Hardness | 1700 | HV 0.5 | |
Thermal Characteristics | Coefficient of Line Thermal Expansion | 2 | 10-6 K-1 |
Thermal Conductivity | 20 | W/mK | |
Thermal Shock Resistance (Put in Water) | 750 | ΔT℃ | |
Max Working Temperature | 1300 | ℃ | |
Electrical Characteristics | Volume Resistance at 20℃ | >10⒕ | Ωcm |
Dielectric Strength | 10×106 | V/m | |
Dielectric Constant | - | εr | |
One MHZ Dielectric Loss Angle at 20℃ | - | tanδ | |
Chemical Characteristics | Nitric Acid(60%)90℃ | 1 | WT Loss mg/cm2/day |
Sulphuric Acid(95%)95℃ | ≒0.00 | ||
Caustic Soda(30%)80℃ | 0.2 |
This data is the result of laboratory testing. Customers need to judge whether it can be used according to the specific environment.
For more customization details, Please contact us.
Silicon Nitride (Si3N4) has the most versatile combination of mechanical, thermal, and electrical properties of any advanced ceramic material. It is a high performance advanced ceramic that is extremely hard and has exceptional thermal shock and impact resistance. It surpasses the high temperature capabilities of most metals and has a superior combination of creep and oxidation resistance. Additionally, its low thermal conductivity and high wear resistance make it an excellent material that can withstand the toughest of conditions in the most demanding industrial applications. Silicon Nitride is an excellent choice when high-temperature and high-load abilities are needed.
Silicon nitride ceramic square structural parts are very wear-resistant because of their superb hardness and self-wetting properties. In addition, silicon nitride ceramic does not react with other inorganic acids except hydrofluoric acid, and is highly resistant to corrosion. Moreover, it has excellent resistance to thermal shock and will not rupture when heated to 1000°C in air and then rapidly cooled.
Silicon Nitride Applications | |
|
Property | Item | Data | Unit |
Mechanical Characteristics | Color | Black/Grey | - |
Density | 3.2 | g/cm3 | |
Bending Strength | 750 | MPa | |
Compressive Strength | 3800 | MPa | |
Elastic Modulus | 290 | GPa | |
Fracture Toughness | 7 | MPa m1/2 | |
Weber Coefficient | 15 | m | |
Vickers Hardness | 1700 | HV 0.5 | |
Thermal Characteristics | Coefficient of Line Thermal Expansion | 2 | 10-6 K-1 |
Thermal Conductivity | 20 | W/mK | |
Thermal Shock Resistance (Put in Water) | 750 | ΔT℃ | |
Max Working Temperature | 1300 | ℃ | |
Electrical Characteristics | Volume Resistance at 20℃ | >10⒕ | Ωcm |
Dielectric Strength | 10×106 | V/m | |
Dielectric Constant | - | εr | |
One MHZ Dielectric Loss Angle at 20℃ | - | tanδ | |
Chemical Characteristics | Nitric Acid(60%)90℃ | 1 | WT Loss mg/cm2/day |
Sulphuric Acid(95%)95℃ | ≒0.00 | ||
Caustic Soda(30%)80℃ | 0.2 |
This data is the result of laboratory testing. Customers need to judge whether it can be used according to the specific environment.
For more customization details, Please contact us.